If fill temperature exceeds the PP grade limits and cooling is rapid/uneven, deformation increases. Use a higher heat-resistant PP grade, add base doming and ribs to boost stiffness, and allow a brief “relax/cool” period before stacking. For very hot products, evaluate alternative materials such as CPET.